Modelling hydrogen induced stress corrosion cracking in austenitic stainless steel

10/16/2019
by   E. I. Ogosi, et al.
0

A model has been developed which simulates the deformation of single crystal austenitic stainless steels and cap-tures the effects of hydrogen on stress corrosion cracking. The model is based on the crystal plasticity theory which relates critical resolved shear stress to plastic strain and the strength of the crystal. We propose an analytical repre-sentation of hydrogen interactions with the material microstructure during deformation and simulate the effects hydrogen will have on void growth prior to fracture. Changes in the mechanical properties of the crystal prior to fracture are governed by the interaction of hydrogen atoms and ensembles of dislocations as the crystal plastically deforms and is based on the hydrogen enhanced localised plasticity (HELP) mechanism. The effects of hydrogen on void growth are considered by analysing the effect of hydrogen on the mechanical property of material bound-ing an embedded void. The model presented has been implemented numerically using the User Material (UMAT) subroutine in the finite element software (ABAQUS) and has been validated by comparing simulated results with experimental data. Influencing parameters have been varied to understand their effect and test sensitivities.

READ FULL TEXT

page 8

page 10

research
11/10/2020

Interaction of void spacing and material size effect on inter-void flow localisation

The ductile fracture process in porous metals due to growth and coalesce...
research
01/11/2020

Continuum modelling of stress diffusion interactions in an elastoplastic medium in the presence of geometric discontinuity

Chemo-mechanical coupled systems have been a subject of interest for man...
research
10/15/2019

Hydrogen Effect on Plastic Deformation and Fracture in Austenitic Stainless Steel

The effect of hydrogen on the fracture behaviour of austenitic stainless...
research
05/31/2022

Deformation of the myocardium during CPR

Cardiopulmonary resuscitation (CPR) is an emergency procedure performed ...
research
10/12/2020

Cyclic Energy Storage in Salt Caverns: nonlinear finite-element modelling of rock salt creep at reservoir scale

Subsurface formations provide giant capacities for renewable energy stor...

Please sign up or login with your details

Forgot password? Click here to reset